42.1 Environmental Effects on Masonry

Key Takeaways

  • Michigan lists severe weathering. Apply the referenced unit standard for grade and use the separate foundation-depth provision.

  • C216-13 SW and MW are weathering grades. Check individual and average criteria and the applicable acceptance path.

  • The saturation coefficient divides cold-water absorption by boiling absorption. IRA measures the speed of early suction.

  • Control saturation, identify moisture paths behind recurring efflorescence, and build compatible movement joints.

  • TMS 602-13 construction thresholds use ambient conditions. Its cold protection thresholds use the forecast minimum for grouted work and mean for ungrouted work.

Last updated: November 2026

Quick Answer: Michigan lists severe weathering. Select masonry units for the material, its standard and the actual exposure. Limit water entry and give the assembly a way to drain. For work under TMS 602-13, use the ambient conditions to plan laying and temperature control, then use the applicable forecast to plan protection after placement.

Michigan exposure: units, water and frost

Rule 516 amends 2015 Michigan Residential Code Table R301.2(1). It lists severe in the weathering column. Footnote (a) sends the installer to the applicable masonry unit standard listed in Chapter 44 to determine grade. The 42-inch entry concerns foundation depth and is subject to Rule 522, including its provision for approved modifications based on site conditions. Footing depth controls exposure to frost-related ground movement. The unit grade addresses durability in service.

Masonry exposed to rain, soil moisture or poor drainage may stay wet long enough to freeze while saturated. Water expands by roughly 9% as it freezes. Ice formation and pressure in wet pores can crack the unit or cause scaling and spalling. A strong unit can still take up water, so check material durability as well as load requirements. Reduce wetting with the relevant flashing, weeps, sloped sills or copings and maintained drainage. Apply the foundation dampproofing or waterproofing detail required for the site.

Clay brick and concrete block

R606.2.2 references ASTM C216-13 for solid facing brick and specifies other standards for other clay unit types. For a facing brick exposed to freezing while wet, such as exterior facing brick in contact with earth, Grade SW specifies high resistance to freeze-thaw damage. Grade MW is intended for exposure where moderate resistance is sufficient. C216-13 includes SW and MW. The grade and a facing brick’s appearance type answer different questions.

C216-13 Table 1 limitsGrade SWGrade MW
Minimum gross-area compressive strength, average of five / individual3,000 / 2,500 psi2,500 / 2,200 psi
Maximum 5-hour boiling absorption, average of five / individual17% / 20%22% / 25%
Maximum saturation coefficient, average of five / individual0.78 / 0.800.88 / 0.90

Read these as the baseline table criteria. C216-13 also has absorption and freeze-thaw alternatives under specified conditions. A coefficient alone cannot qualify a shipment. Apply the complete applicable acceptance path and obtain supplier documentation.

The saturation coefficient is 24-hour cold-water absorption divided by 5-hour boiling absorption. For two individual test specimens, 12.0 ÷ 16.0 = 0.750 and 14.0 ÷ 16.0 = 0.875. The first is within the 0.80 individual SW coefficient limit. The second exceeds that limit and is within the 0.90 individual MW limit. Both have 16% boiling absorption. Check the other properties, the five-unit averages and any applicable alternate path before judging conformance. Keep extra precision during comparisons.

Initial rate of absorption (IRA) measures how rapidly the bed face draws water at first contact. It differs from total absorption or the saturation coefficient. High suction can remove water from the mortar before a good bond develops. Under TMS 602-13 Article 3.2 A, wet clay or shale units with an ASTM C67 IRA over 1 g/min per in², equivalent to 30 g/min per 30 in², to bring the rate within that limit when laid. The wetted units must be surface dry when laid. Routine prewetting does not apply to concrete masonry or AAC units under that specification unless otherwise required.

R606.2.1 references ASTM C90-13 for load-bearing concrete masonry units. In that edition the net-area strength minima are 1,900 psi for the three-unit average and 1,700 psi for an individual unit. The 2014 revision raised the average minimum to 2,000 psi. Check the contract and code-referenced date before using a newer value. Concrete masonry unit strength, mortar strength and assembly strength describe different tests. Nonload-bearing units under ASTM C129 serve a different use. Specify drying-shrinkage and other unit properties under the applicable standard and job requirements.

Diagnose moisture, salts and movement

Efflorescence forms when soluble salts, moisture and a route to a drying surface coincide. Water transports dissolved salts through pores, across surfaces or along a joint. Evaporation leaves a powdery deposit. Construction moisture can cause an early bloom. Repeated deposits near sills, at ground level or below an opening warrant checking the local moisture path, such as a flashing lapse, plugged weep or poor drainage. For loose deposits, begin with dry brushing using a nonmetallic brush. Confirm the type of stain and use a compatible cleaning method. Control the moisture and salt sources to limit recurrence.

Sulfate exposure from soil or groundwater can deteriorate cementitious materials. Some reactions form expansive products such as ettringite, leading to cracking and scaling. Identify the exposure and specify compatible cementitious materials and water control. Efflorescence is a surface deposit and does not by itself establish sulfate attack.

Movement can crack an otherwise sound wall when restrained. Fired clay brick tends to expand over time as it takes up moisture. Concrete masonry tends to shrink as it dries. Both also respond to temperature changes. Use designed expansion or control joints, coordinated with the backing and veneer supports. Keep the separation and sealant detail free of unintended rigid bridges.

Weather during and after masonry work

For work governed by TMS 602-13 Article 1.8, distinguish the ambient air at the work from the forecast used to protect finished work. Below 40°F ambient, apply the cold-weather procedure. Do not lay units below 20°F or with frozen moisture, visible ice or snow. Where new work bears on an existing foundation or masonry in these conditions, remove visible ice and snow and bring the receiving surface above freezing without damage. The glass-unit and thin-bed AAC provisions have separate requirements.

Ambient air while layingCold-weather construction checks for conventional masonry
Below 40°F down to 32°FHeat sand or mixing water to make mortar 40–120°F at mixing. Heat grout materials if their own temperature is below 32°F.
Below 32°F down to 25°FHeat both mortar sand and water and keep mortar above freezing until used. Produce grout at 70–120°F at mixing and keep it above 70°F at placement.
Below 25°F down to 20°FContinue the preceding measures, heat masonry surfaces to at least 40°F, including before grouting, and provide a windbreak or enclosure when wind exceeds 15 mph.
Below 20°FContinue the preceding measures and enclose and heat the work space above 32°F.

During cold work keep the water and aggregates used in mortar or grout at or below 140°F. This is a limit on heated components. Check the separate temperatures of the mixed materials.

For post-placement conventional masonry protection, use the forecast minimum for grouted masonry and mean for ungrouted masonry. From 40°F down to 25°F, provide weather-resistant covering for 24 hours. Below 25°F down to 20°F, use complete insulating protection for 24 hours. Below 20°F, keep the new work above 32°F for at least 24 hours. In the latter two bands, extend the protection to 48 hours for grouted masonry unless Type III portland cement is the only cement in the grout. Also protect unfinished wall tops from water intrusion.

Hot-weather construction starts when ambient air exceeds 100°F, or exceeds 90°F with wind over 8 mph. Keep sand damp and loose and keep mortar and grout below 120°F during work. Cool the mixer, transport containers and mortar boards with water before contact with the mix. Keep mortar workable by permitted retempering with cool water and use it within two hours of initial mixing. When ambient air exceeds 115°F, or exceeds 105°F with wind over 8 mph, also shade materials and mixing equipment and use cool mixing water. Ice used to cool the water must melt before the water is added.

After installation, use the hot-weather mean daily trigger of over 100°F, or over 90°F with wind over 8 mph. Fog the new work until damp at least three times per day until the masonry is three days old. Keep this curing measure separate from any prewetting required for high-suction clay units.

Jobsite example. A wall is laid at 37°F with grout ingredients held at 35°F. The below-40°F work procedure applies, but this temperature band does not impose the colder band's 70°F grout-mixing minimum. If the grouted wall's forecast low is 22°F and the grout does not use only Type III portland cement, protect it with insulation or an equivalent for 48 hours after completion. These are two independent decisions.

Test Your Knowledge

A Michigan project specifies solid facing brick in contact with earth where wet brick is exposed to cyclic freezing. Which ASTM C216-13 grade addresses the intended severe exposure?

A

Grade MW, because moderate resistance is intended for saturated freeze-thaw exposure

B

Grade NW, because it is a C216-13 facing-brick grade for decorative masonry

C

Grade SW, because that grade targets high resistance to freeze-thaw damage

D

Type FBX, because tight dimensional tolerances establish freeze-thaw resistance

Test Your Knowledge

One brick has 12.0% absorption in the 24-hour cold-water test and 16.0% in the 5-hour boiling test. What does its result show under the ASTM C216-13 Table 1 route?

A

The coefficient is 0.750, within the 0.80 individual SW limit. Additional results are needed for grade conformance.

B

The coefficient is 1.333 and misses the individual SW limit.

C

The coefficient is 0.040, found by subtracting the cold result from the boiled result.

D

The coefficient is 0.750, enough on its own to approve the shipment as Grade SW.

Test Your Knowledge

A crew lays conventional grouted masonry under TMS 602-13 in 37°F ambient air. The forecast minimum after placement is 22°F and the grout uses Type I portland cement. What post-placement protection does this forecast require?

A

A weather-resistant membrane for 24 hours without insulation

B

Complete insulating protection or an equivalent for 48 hours

C

A heated enclosure holding the masonry above 32°F for only 24 hours

D

No protection as long as the ambient temperature while laying was above 32°F