31.3 Concrete Characteristics & Types
Key Takeaways
ASTM C143 measures fresh concrete consistency. Prescriptive foundation-wall slump has a 6-inch removable-form limit with an approval exception and must exceed 6 inches in stay-in-place forms. Internal vibration is the default for stay-in-place forms.
Concrete has relatively low tensile capacity. For normal-weight concrete, ACI 318 estimates the modulus of rupture at about 7.5 times the square root of specified compressive strength in psi.
Entrained air improves freeze-thaw and deicer scaling resistance. Michigan uses the severe weathering column of Table R402.2, with specific concrete locations and air-content conditions.
Shrinkage can occur without load. Creep is time-dependent deformation under sustained load. At an assumed free shrinkage strain of 0.05%, a 10-foot length shortens about 1/16 inch.
Select lightweight concrete for reduced dead load, a high-early-strength mix when early strength matters, a specified fiber dosage for crack control, and self-consolidating concrete for flow without conventional vibration.
Quick Answer: Evaluate fresh concrete for placement and hardened concrete for strength, stiffness and exposure. Select the mix and acceptance tests for the assembly.
Fresh concrete: what the crew can see
Workability is how readily a mix can be placed, consolidated and finished while remaining cohesive. ASTM C143 slump measures consistency. The 12-inch cone has an 8-inch base and 4-inch top. Fill it in three layers of approximately equal volume, rod each 25 times, strike off, remove the cone vertically and measure the drop at the displaced original center of the top surface.
Select the specified slump for the mix, placement method and reinforcement conditions. A low-slump mix may suit open footing forms. Congested reinforcement and pumping often call for more flow. A water reducer can raise slump at the same w/cm. Evaluate strength and air content separately.
Foundation walls: Under MRC R404.1.3.3.4, removable forms normally have a 6-inch maximum. A higher slump needs approval for a segregation-resistant mix consistent with the form manufacturer’s recommendations. Stay-in-place forms require slump greater than 6 inches and, under .5, internal vibration. The no-vibration exception requires approval for a self-consolidating mix specifically designed for placement without internal vibration and with slump of at least 8 inches. MRC R608.5.1.4 and .6 address the analogous concrete-wall rules. Where specified for SCC, ASTM C1611 measures slump flow, the horizontal spread, which is a different value from vertical slump.
Cohesion helps keep the coarse aggregate distributed in the mortar. Aggregate piles at discharge or mortar-starved rock pockets in the forms can indicate segregation. Control the discharge, check mixture stability and use the prescribed consolidation technique.
Bleeding is water rising as solids settle. Wait for free surface water to disappear before final finishing. Excess bleed water can bring fine material to the surface, and working that water into the surface weakens the paste and contributes to dusting or scaling. Finishing too early can also trap bleed water and air under a dense surface.
Setting time depends on concrete temperature, cementitious materials and admixtures. Hot, dry and windy conditions can draw water from the surface faster than bleeding replaces it, producing plastic shrinkage cracking while the mix is still fresh. Plan evaporation control and finishing and curing around the actual conditions.
Hardened concrete: strong in compression, weak in tension
Compressive strength is measured by testing cylinders under ASTM C39. Acceptance specimens are made and standard-cured under ASTM C31 when specified for the work, then tested at 28 days or the specified age. Early breaks show how that sample is developing. They cannot fix a later strength value or establish the in-place strength required for form removal.
Concrete has much less capacity in tension than in compression. For normal-weight concrete, ACI 318 estimates its flexural tensile strength (modulus of rupture) in psi as , using specified compressive strength in psi. Deformed reinforcement transfers tension through bond once the concrete cracks. A specific fiber system can add crack control or post-crack performance where the design provides for it.
For normal-weight concrete, ACI 318 permits estimating elastic modulus as psi with specified strength in psi. At 3,000 psi that gives about 3.12 million psi, roughly one-tenth of structural steel’s elastic modulus. Time-dependent deformation can increase service deflection further.
Durability
Durability is the ability to survive Michigan weather, and it depends on air content, permeability and chemistry:
- Freeze-thaw. Water in pores expands on freezing, and hydraulic pressures can disrupt the paste. An adequate entrained-air system relieves pressure. Exposure, permeability, curing and deicing salts all influence scaling risk.
- Permeability. A suitable low w/cm and adequate curing can reduce transport of water and chlorides into the concrete.
- Sulfate attack. Sulfates in soil or water can enter the concrete and react with the paste. Check exposure classification and specify a suitable sulfate-resistant binder or verified blend and low permeability.
- Alkali-silica reaction. Available alkalis, susceptible aggregate and moisture can produce an expansive gel. Test the aggregate and use a verified mitigation strategy for those materials and conditions.
- Carbonation. Carbon dioxide reacts with hydrated cement phases and reduces alkalinity. If the carbonation front reaches embedded steel, steel loses its chemical protection. Good cover, low permeability and proper curing help slow penetration.
Shrinkage, thermal movement and creep
Drying shrinkage results from moisture loss from the hardened paste. Actual strain depends on aggregate, paste, curing, humidity and member geometry. For a free-shrinkage example, 0.05% × 120 in = 0.06 in, close to 1/16 inch per 10 feet. At that same strain over 100 feet, free movement would be 0.6 inch. Restraint can turn shrinkage into cracking, which the joint and reinforcement design addresses.
Plastic shrinkage happens before hardening when evaporation at the surface outpaces bleeding. Windbreaks, shade, fogging where appropriate and timely curing reduce risk. Extra batch water can weaken the surface and does not address evaporation.
Thermal movement depends on the mixture and change in temperature. With an assumed coefficient of 0.000006 per °F, a free length of 100 ft × 12 in/ft × 0.000006/°F × 50°F changes by 0.36 inch. The joints and restraints determine how that movement is accommodated.
Creep is time-dependent deformation under sustained load. It can partially relieve restrained shrinkage stress, increase long-term beam deflection and contribute to loss of prestress. Its magnitude depends on loading age, sustained stress, the mixture, member size and environment.
Types of concrete and when each is specified
| Type | What it is | Selection and checks |
|---|---|---|
| Normal-weight | Typically about 140 to 150 lb/ft³ with ordinary aggregates | Common for footings, walls and slabs. Verify actual density where needed. |
| Structural lightweight | Uses qualifying lightweight aggregates such as ASTM C330 materials | Reduce dead load. Verify equilibrium density, strength and stiffness. |
| High-early-strength | Mix proportioned for rapid strength development, for example with Type III cement or an accelerator | Check in-place strength for early stripping or loading. |
| High-strength | In ACI terminology, specified design strength of at least 8,000 psi | Check mixture qualification, testing and curing for the structural application. |
| Fiber-reinforced | Uses a specified steel, synthetic or other fiber system | Fibers can control early cracking or provide designed residual capacity, depending on type and dosage. Check structural reinforcement requirements. |
| Self-consolidating | Formulated for stable flow around obstructions and consolidation without conventional vibration | Verify flow, segregation resistance, approvals and form pressure. |
| Air-entrained | Microscopic air void system for freeze-thaw and scaling resistance | Check the applicable total-air range and the actual fresh properties. |
| Colored or stamped | Uses pigments and/or tools to texture the surface | Choose products, finishing and maintenance for the exposure. |
| Pervious | Open aggregate structure with little or no fine aggregate | Allows stormwater through; confirm drainage design, soil compatibility, structural capacity and maintenance. |
Putting the types to work on one house
A house with ICF basement walls, a garage and an interior basement slab needs three separate checks. Specify the ICF wall slump and internal consolidation under R404.1.3.3.4 and .5, or obtain approval for a qualifying self-consolidating mix. A typical Michigan garage slab takes 3,500 psi and 5% to 7% total air under Table R402.2. A steel-troweled garage floor may use the table’s 4,000 psi and at least 3% air option. The basement slab has a 2,500 psi baseline, with air required if subject to freezing and thawing during construction under the table’s footnote, and the specified retarder under R506.2.3 where required.
Order each mix by its approved designation, then check the delivery ticket and specified tests before incorporating it into the applicable assembly.
What property of fresh concrete does the standard slump test measure?
The compressive strength the mix will reach at 28 days
The consistency of the fresh mix
The total air content of the mix
The initial and final setting time of the concrete
What is the purpose of air entrainment in the concrete for a Michigan garage floor exposed to freeze-thaw and deicing salts?
It increases compressive strength so a leaner mix can be used
It speeds up initial set so the slab can be finished sooner
It reduces drying shrinkage and eliminates the need for contraction joints
It provides microscopic relief voids that improve resistance to freeze-thaw damage and scaling
Sections you finish are checked off in the contents.