42.3 Jointing & Mortar Joints

Key Takeaways

  • R606.3.1 sets the default ⅜-inch bed and head joint and a ¼- to ¾-inch starting bed over the foundation.

  • Solid masonry and hollow masonry have different fill requirements. Check specified cross webs around partially grouted cells.

  • BIA recommends compacted concave, V and grapevine profiles for exposed brickwork. Keep drainage details functional.

  • Tool when the mortar is thumbprint hard and still responds to pressure.

  • Repoint historic joints with a compatible mortar and profile after investigating the source of deterioration.

Last updated: November 2026

Quick Answer: Fill the required bedding and head-joint areas and tool the specified profile when the mortar is firm enough to hold a thumbprint. A compacted, concave, V or grapevine detail is a common water-resistant choice for exposed brick. Give the wall its own flashing and drainage where the assembly calls for it.

Know which surfaces need mortar

A bed joint is horizontal and supports a course. A head joint is between units in the same course. A collar joint runs vertically between wythes and may receive mortar or grout where indicated by the assembly design. A drainage space in anchored veneer must remain clear enough to drain.

Under the prescriptive 2015 MRC R606.3.1, the usual bed and head joint thickness is ⅜ inch unless otherwise required or shown. The starting bed on the foundation has its own range of ¼ to ¾ inch. Inspect load-bearing joint tolerances against the specified dimensions and the applicable provision. Do not infer a universal tolerance for all three joint types from the nominal thickness.

Fill the joints that the design requires. Under R606.3.2.1, solid units get full head and bed joints, plus filled interior vertical joints where designed to receive mortar. Under R606.3.2.2, fill the head and bed joints of hollow units from the face inward at least the face-shell thickness. In a partially grouted wall, also bed the cross webs enclosing the cells to be filled. Incomplete face-shell or head joints can leave water paths even when the outside has been dressed. Use enough pressure to close the joint as the unit is placed. Deep furrows that leave voids are prohibited.

Choose and form the profile

ProfileFormationSelection for exposed brick
ConcaveRounded tool presses a shallow curved recessA common durable choice that compacts the exposed mortar
VTool presses a V-shaped grooveCompacted detail when the design calls for a sharper line
GrapevineTool forms a narrow groove in the faceAnother water-resistant detail when properly compacted
Weathered and struckSloped faces with opposite orientationsCheck the specified slope, edge and compaction. BIA favors compacted profiles for exposed brick.
FlushFace dressed even with the unitsUseful where a flat face is needed, such as a specified base for a finish
RakedMortar recessed to a set depthRecess can leave a ledge or insufficiently compacted face. BIA generally advises against using it for exposed brick.
Beaded or extrudedRaised decorative profile, or excess mortar allowed to projectIn exposed work, check the design and exposure. Projecting material or incomplete compaction can reduce durability.

Weather-resistant tooling presses the mortar against the adjoining faces and consolidates the exposed surface. Concave, V and grapevine profiles are recommended for exterior brickwork in BIA Technical Note 7B. Those recommendations help select a joint profile. The structural bedding provisions still apply. With historic work, retain the original character where it can be made serviceable. Avoid changing a specified profile solely for appearance.

Time tooling by mortar condition

Tool when the joint is thumbprint hard. A thumb leaves a clear impression without pulling wet material out. The mortar should still respond to the tool's pressure. A fixed number of minutes is unreliable because temperature, wind and the unit's absorption change when the joint is ready.

  • If the mortar is wet, the tool can smear the edges and the joint may shrink back from the units. Check a small area first.
  • If the mortar has hardened too far, tooling no longer closes the joint well and may mar its color or edges. Adding wet mortar over an unsuitable joint does not restore the underlying bond.
  • Use the jointer appropriate to the profile and finish at a consistent condition and pressure. Tool the head and bed joints and remove crumbs with a suitable brush once the joint can withstand it.

In exposed anchored veneer, verify flashing and open weeps at the required drainage points. Keep mortar from bridging the drainage path. Follow the specified water-resistive layer and flashing lap. Sloped sills and copings reduce direct wetting. Avoid treating a fine-looking joint as proof that the concealed water management was installed.

Repoint existing masonry

Repointing replaces deteriorated joint mortar. In preservation work, tuckpointing can refer to a decorative contrasting line added to the joint, although the word is also used for repointing in ordinary trade speech. Diagnose the water source and the condition of the units and historic mortar before setting the repair scope.

National Park Service Preservation Brief 2 recommends removing loose, deteriorated mortar to a minimum depth on the order of 2 to 2½ times the joint width, and deeper where loose material remains. In a ⅜-inch joint this gives ¾ to 15/16 inch. Clear debris without damaging unit edges. Dampen absorptive surfaces as appropriate and let free water dissipate before placing mortar. Pack the back of the joint and build up in controlled layers. Tool the final layer at thumbprint hardness to match the sound historic work, then protect it for the specified cure.

The preservation mortar should be softer and more vapor permeable than the masonry units and at least as permeable and as soft as the sound historic mortar. Strength and permeability must be checked separately. A hard and less permeable replacement can contribute to damage in a soft brick or stone. Determine the appropriate composition, sand, color and profile from the existing work and exposure. A type letter alone cannot establish compatibility.

Inspect the work

Check the joint fill before it is concealed. On hollow units confirm continuous bedding where the shells and any required webs bear. Check joint size against the applicable detail, the face for compact tooling and the drainage path for mortar blockage. Investigate cracks and recurring deposits before choosing a repair. Repointing replaces deteriorated mortar within the joint. A specified sealant in a movement joint serves a different function.

Test Your Knowledge

For an exposed clay brick wall, which of the listed details follows BIA water-penetration guidance for a compacted outer joint?

A

An untooled raked joint with a horizontal ledge

B

A flush-cut joint with the exposed mortar left uncompacted

C

A projecting bead left untooled

D

A tooled concave joint compacted against the units

Test Your Knowledge

When should a crew tool its bed and head joints for the specified compacted profile?

A

While the mortar is wet enough to smear onto the unit face

B

After the mortar has cured

C

At thumbprint hardness, while the joint still responds to tool pressure

D

After the wall has been washed

Test Your Knowledge

Under prescriptive 2015 MRC R606.3.1 with no different specified joint size, what is the ordinary bed and head joint thickness and the permitted starting bed thickness over a foundation?

A

½ inch, with a ⅜- to 1-inch starting bed

B

¼ inch, with a ¼- to ½-inch starting bed

C

⅜ inch, with a ⅜- to ¾-inch starting bed

D

⅜ inch, with a ¼- to ¾-inch starting bed

Sections you finish are checked off in the contents.