8.1 Identifying Steels, Aluminum and High-Temperature Alloys

Key Takeaways

  • Many conventional SAE numbers identify an alloy family and a nominal carbon level. The specification and material report establish the actual limits and condition.

  • Annealed 304 and 316 are austenitic. Cold work and material condition can change their magnetic response and machining behavior.

  • A wrought aluminum designation identifies an alloy group, and its suffix identifies the temper. Check both against the drawing.

  • Start from the toolmaker’s recommendations for the exact alloy, condition and operation, especially for titanium and nickel superalloys.

Last updated: November 2026

8.1 Identifying Steels, Aluminum and High-Temperature Alloys

Identify both the grade and condition

Ferrous alloys are iron-based. Nonferrous alloys are based on another metal and may still contain some iron. Match the material tag or traceable job record to the required grade, product form and condition. Do this before selecting stock or loading a previous setup. A successful cut on annealed stock does not establish that its tooling suits a hardened lot of the same nominal grade.

Conventional SAE numerical grades are shorthand for ranges of composition. In many four-digit designations the first pair identifies a chemistry family and the last pair indicates approximate nominal carbon in hundredths of a weight percent. For example, 4140 identifies a chromium-molybdenum alloy steel with a nominal carbon level near 0.40%. Actual limits depend on the specification and product form. The digits do not tell you the delivered hardness. SAE's newer alphanumeric framework coexists with older familiar numbers; use the specification on the job.

Familiar grade or familyHow to interpret it for a job
1018 and 1045Conventional carbon-steel examples. Their nominal carbon levels differ. Obtain the supplied condition before deciding whether a feed or edge preparation can be carried over.
1215 and 12L14Examples supplied as free-machining steel. 1215 is rephosphorized and resulfurized. 12L14 includes a deliberate lead addition. Where the job restricts lead or alloy substitution, check the material specification and the shop's controls.
4140 and 4340Alloy-steel examples. 4140 uses chromium and molybdenum; 4340 adds nickel to a chromium-molybdenum alloy system. Choose tooling using the actual stock condition.
8620Nickel-chromium-molybdenum low-alloy steel used for carburized parts. An as-supplied blank and a finished carburized surface can present different machining conditions.

Free-machining additions can improve chip control and tool life in suitable operations. Manganese sulfide inclusions are relevant to resulfurized steels. A substitution between free-machining grades can change chemistry and other part requirements even when a test cut looks similar. Check the drawing and approved material route.

Identify the stainless-steel family

Chromium-rich passivation gives stainless steel its corrosion resistance. The family and supplied condition affect the machining approach.

Example familyExamplesShop consequence
Austenitic304, 316Conventionally solution annealed material is generally nonmagnetic, and some grades can become magnetic after cold work. Choose an edge/feed combination that cuts rather than rubs.
Ferritic430Ferritic structure is generally magnetic. Match the specific grade and cutting operation.
Martensitic410, 440CHeat treatment can harden these alloys. Identify whether the surface is in the intended pre- or post-hardening condition.
Duplex2205A mixture of austenite and ferrite. Use the toolmaker's duplex data for the exact cut.
Precipitation-hardening grades17-4 PHThe delivered or aged condition matters. Use the required condition, rather than assuming all PH alloys share one microstructure or hardness.

Austenitic 304 and 316 can strain harden under deformation. A dull edge, rubbing cut or unplanned dwell can leave a hardened area for the next pass. Diagnose the cut with the tool supplier's recommendations and observed load, wear and finish. Neither a universal minimum chip load nor a fixed fraction of heat at the tool applies to every setup.

Decode wrought aluminum and identify the high-temperature alloy

For wrought products, the Aluminum Association's first digit identifies a family. 1xxx is at least 99% aluminum, 2xxx is copper-based, 3xxx manganese, 4xxx silicon, 5xxx magnesium, 6xxx magnesium and silicon, 7xxx zinc and 8xxx other elements. This rule is for the written wrought designation. Cast alloys use a different system. The suffix is separate. O indicates annealed, T4 solution heat treated and naturally aged, and T6 solution heat treated and artificially aged. For an applicable T651 product, controlled stretching relieves residual stress. That lowers a source of distortion while cutting. Moving material away from a thin wall may still release stresses or expose poor support.

Grade 5 Ti-6Al-4V is an aluminum- and vanadium-bearing titanium alloy. Low thermal conductivity can lead to high local cutting temperatures. A stiff setup, appropriate edge and the toolmaker's material-specific cutting data matter. INCONEL alloy 718 is a precipitation-hardenable nickel-chromium alloy; check its condition and choose data for the actual HRSA operation. Room-temperature property data do not specify turn or mill settings.

Apply the receiving check to a real setup

A print calls for 6061-T651 plate for a pocketed bracket. The rack contains 6061-T6 and 7075-T651. Both labels share one field with the print. Hold substitution for approval and locate the correct plate and material record. Confirm flat seating before and after roughing, and check the thin wall in the required free or restrained state. This separates alloy and temper verification from machining behavior and final inspection.

SAE steel designations, SAE carbon grade chemistry, Outokumpu stainless families, Aluminum Association wrought designations, ATI Grade 5 Special Metals alloy 718 and Sandvik titanium cutting guidance

Loading diagram...
Read the material record before selecting cutting data
Test Your Knowledge

In conventional SAE 4140, what can be inferred from the last two digits?

A

A nominal carbon level near 0.40% by mass

B

A finished hardness of 40 HRC

C

An exact chromium concentration of 0.40%

D

A specified tempering temperature of 400°F

Test Your Knowledge

A lot of cold-worked stock marked 304 attracts a magnet. How should the operator confirm whether it is the correct material?

A

Reject it based only on the observed magnetism

B

Accept it as 440C because all magnetic steel is martensitic

C

Check the traceable material record and condition because some cold-worked austenitic grades can respond to a magnet

D

Compare only its color to a known sample

Test Your Knowledge

What alloying elements identify the 6xxx family in the wrought aluminum designation system?

A

Copper and zinc

B

Magnesium and silicon

C

Manganese and zinc

D

Silicon and chromium

Test Your Knowledge

The previous titanium job used a rigid short carbide cutter. A new cut on the same grade needs a long reach. What evidence should set the new starting conditions?

A

Use the documented short-tool run and adjust only its spindle speed.

B

Select cutting data from any carbide tool of the same diameter and flute count.

C

Reuse the earlier chip load and establish speed from the machine limit.

D

Use toolmaker data for this alloy, cutter, reach and operation.

Sections you finish are checked off in the contents.