4.1 Cutting Tool Materials and Coatings
Key Takeaways
Identify the work material and condition before choosing a grade. ISO 513 application groups organize the search, and the supplier’s material subgroup and application data narrow the choice.
Select the substrate for the combination of edge toughness, hot hardness, chemical compatibility and wear resistance. The right combination depends on the cut.
PVD grades often suit sharp, tough cutting edges. CVD grades offer wear resistance and may also be suitable for milling, depending on the grade.
PCD is a composite with excellent abrasion resistance for suitable nonferrous work. Diamond loses chemical stability in hot contact with iron.
4.1 Cutting Tool Materials and Coatings
Start with the cut
A grade is the manufacturer’s particular combination of substrate and, when used, coating. The edge geometry adds another choice. A thin wall calls for a freely cutting edge because the part can deflect. An interrupted cut calls for an edge that can withstand repeated entries. A long, steady run in abrasive stock may make gradual wear more important than impact resistance. Several tools can fit the pocket in a holder and still behave very differently in the cut.
Hot hardness is resistance to softening while hot. Wear resistance extends the useful cutting edge under abrasion or chemical attack. Toughness helps prevent chips or larger fractures in the tool itself. Compare all three and check how the proposed cutting edge interacts with the specific material, including its hardness and surface condition.
Substrate families
| Family | Where it can fit | What to check before substituting |
|---|---|---|
| High-speed steel (HSS) | Drills, taps and form tools where toughness and a sharpenable edge matter | Use the speed data for the actual HSS tool. Böhler lists 8% cobalt for its M42-family S500 grade. Cobalt-bearing HSS improves hot hardness. |
| Cemented carbide | Broad use in solid cutters and indexable inserts | Sintered tungsten carbide particles and a cobalt-rich binder provide a balance of hardness and toughness. At comparable grain size, a higher binder content generally increases toughness and reduces resistance to plastic deformation. Finer WC grains can increase hardness at a given binder content. |
| Cermet | Stable finishing cuts in suitable steels when surface finish and resistance to adhesion are important | Titanium carbonitride-based grades offer low smearing tendency. Verify minimum depth and feed and the grade’s suitability for interruptions. |
| Ceramic | Selected high-speed machining with suitable grades and rigid setups | Alumina-based and silicon nitride-based grades have different uses. Mixed or whisker-reinforced alumina grades can suit specific hard-turning or superalloy cuts. Silicon nitride grades are used in suitable gray cast iron work and have limited chemical stability in steel. |
| Cubic boron nitride (CBN) | Finish turning of hardened steels in an approved hardness range | Buy the grade for the hardness and interruption. Check the edge preparation and cooling guidance. Small CBN tips and different binder systems have different behavior. |
| Polycrystalline diamond (PCD) | Abrasive nonferrous materials, especially high-silicon aluminum, and some composites | PCD consists of diamond particles sintered with a binder. Avoid selecting it for steel cutting. Diamond is chemically unstable in hot contact with iron. For conventional steel machining, look up an approved carbide, ceramic or CBN grade for the condition. |
Read application group and grade separately
ISO 513:2012 organizes hard cutting materials by application. The application marking points to an intended group. It does not specify the composition of a supplier’s carbide. A catalog can describe different grades for the same group and recommend one grade across several groups.
| Group | Catalog color | Typical work material to look up |
|---|---|---|
| P | Blue | Carbon and alloy steels |
| M | Yellow | Stainless steels, including austenitic and duplex grades |
| K | Red | Cast irons, including gray and nodular irons |
| N | Green | Nonferrous metals such as aluminum, copper and brass |
| S | Orange | Nickel- and cobalt-based heat-resistant alloys and titanium alloys |
| H | Gray | Hardened materials such as hardened steel and chilled cast iron |
Supplier subgroup and hardness matter near group boundaries. Match the actual material entry in the chosen catalog. Consult the separate application data for composites. When an older drawing or shop document specifies a U.S. C-grade, use the supplier’s actual cross-reference and verify the cutting conditions. A C-number alone cannot identify an equivalent ISO grade, binder percentage or coating.
What the coating contributes
Chemical vapor deposition (CVD) forms the coating through a chemical reaction. Sandvik’s carbide overview gives deposition temperatures of 700–1,050°C for its CVD discussion. In a modern multilayer coating, titanium carbonitride can improve wear resistance on the flank, and alumina can limit heating of the substrate and improve crater-wear resistance. CVD grades serve general turning and several milling applications. Interrupted cuts require a grade and edge preparation approved for that service.
Physical vapor deposition (PVD) deposits material vapor, sometimes with a reactive gas to form a compound such as a nitride. The same overview gives a 400–600°C deposition range. Compressive stresses in PVD coatings can improve edge toughness. A manufacturer may select PVD for an edge that must stay sharp and endure repeated impacts. Read the supplier’s documentation for the finished edge rather than inferring the edge hone from the coating process.
| Coating name | Useful distinction |
|---|---|
| Titanium nitride (TiN) | Familiar gold-colored coating with broad applications. Color can also serve as a wear indicator in a multilayer system. |
| Titanium carbonitride (TiCN) | In the supplier’s PVD grades, it raises hardness relative to TiN and can improve flank-wear resistance. |
| Titanium aluminum nitride (TiAlN) | Combines hardness and oxidation resistance. Choose a thermal operating window from the actual grade’s data. |
| Aluminum oxide (alumina) | In the named CVD systems it adds a thermal barrier and resistance to crater wear. |
| Diamond-like carbon (DLC) | A family of carbon coatings. For example, Oerlikon specifies its BALINIT MAYURA ta-C coating for eligible nonferrous applications where material adhering to the edge is a concern. |
The temperature in a deposition furnace is different from the service conditions at an edge. Neither process name gives a cutting-speed limit. Coating color, coating thickness and bulk hardness alone cannot identify the right grade.
Distinguish steady wear from edge chipping
Suppose a carbide milling tool develops chips along the edges during interrupted entries in steel. The material narrows the search to an appropriate P application. First inspect the insert seating, workholding, runout and entry conditions. If those conditions are sound, compare a tougher grade and edge preparation specified for interrupted operation. For the same material in a stable run where an approved insert wears gradually at the flank, a wear-resistant grade may extend useful tool life. Keep the candidate grades, shop result and inspection criteria tied to the actual operation.
Sandvik cutting tool materials, work material groups, Böhler grade data and Oerlikon BALINIT MAYURA
Which material is a poor choice for hot cutting contact with carbon steel because diamond loses chemical stability in contact with iron?
Polycrystalline diamond
Cemented carbide intended for steel
Coated high-speed steel
CBN graded for hard turning
An interrupted milling cut requires a sharp edge and resistance to chipping. Which tooling choice is justified?
Use the thickest CVD coating solely because it is thick
Evaluate a sharp PVD grade approved for the cut
Use any grade with a gold surface
Use any grade as long as deposition occurred above 600°C
What application group would you check first for a nickel-based heat-resistant superalloy such as Inconel 718?
P
M
S
H
Why might a manufacturer incorporate alumina in a CVD turning grade for a hot, steady cut?
To turn a soft steel substrate into carbide
To make all inserts suitable for dry cutting
To make the cutting edge center-cutting
To improve crater-wear resistance and provide a thermal barrier
Sections you finish are checked off in the contents.