6.2 Gas Metal Arc Welding (GMAW) Transfer Modes & MCAW
Key Takeaways
Gas metal arc welding uses a continuous consumable electrode and external shielding gas.
Identify transfer from the electrode behaviour, setup and selected program. Change the transfer mode only under the applicable procedure.
Short-circuit transfer repeatedly brings the wire tip into contact with the pool. Spray methods transfer droplets across the arc.
Check the gas identity and shielding conditions at the joint. Porosity can arise from several causes.
Metal-cored electrodes have a tubular sheath and predominantly metallic core. Confirm the qualified product and gas.
Identify the wire, power source and shielding gas
Gas metal arc welding (GMAW) uses an arc between a continuously fed consumable wire and the work, with external shielding gas. Solid wire GMAW does not normally create a heavy slag layer. The feeder, contact tip and gun deliver the wire and gas. Inspect the labels and settings before deciding which wire or transfer mode you are observing.
Many solid-wire applications use constant voltage (CV) with direct current electrode positive (DCEP). On a conventional CV setup, a short-term reduction in arc length tends to increase current, accelerating wire melting and helping restore arc length. The selected wire feed speed, voltage setting and electrical extension affect the actual operating point. Modern waveform-controlled equipment can respond differently. Use the displayed or measured values required by the welding procedure data sheet (WPDS).
Distinguish transfer modes
Metal transfer describes how molten electrode metal enters the pool. An inspector can often identify the selected mode from the procedure and machine setup. Appearance and sound alone can be misleading.
| Transfer | What happens | Inspection point |
|---|---|---|
| Short circuit | The wire repeatedly contacts the pool. The droplet transfers during the short circuit and the arc re-establishes. | Useful for some thin material or open roots. With unsuitable settings or technique, incomplete fusion can occur. |
| Globular | Large drops traverse the arc irregularly. | Check the specified procedure. A globular setup can produce more spatter than an appropriate spray setup. |
| Axial spray | Small droplets are driven along the electrode axis across the arc. | An appropriate shielding gas and a current above the transition for the particular wire and setup support spray. Its fluid pool can restrict positions. |
| Pulsed spray | Current pulses transfer droplets with a lower background current between pulses. | Can allow more positional control than conventional spray. Confirm that the actual waveform or program meets the WPDS. |
A spray transition depends on the wire, diameter, shielding gas and setup. An argon-rich mixture for steel is common. One argon percentage or current threshold cannot identify the mode across applications. Short-circuit transfer is different from using a short stick electrode. Verify whether the specified joint, gas and transfer mode are covered by the approved procedure and whether additional qualification is required. A broad plate-thickness rule cannot replace that check. Lincoln Electric GMAW guide and CWB Form 101E company certification guide.
Worked inspection. A shop WPDS calls for pulsed spray with a specified mixture. The power source is set for a short-circuit program. The cylinder label matches the specified gas. The gas match does not validate the program. Record both facts and identify the affected welds. Verify the approved setup before continuing and obtain disposition for the work already deposited. Internal fusion may require a different examination from the surface condition check.
Follow the shielding gas to the weld
The gas must reach the weld region while it is needed. Check the cylinder or supply label, flow verification method, hoses and nozzle. A blockage or leak can impair delivery, and drafts can displace the shielding at the arc. Excessive turbulence can also entrain air. Compare shielding conditions with the procedure and work instructions. If porosity appears, note when the condition started, where the weld was made and any change in setup. Review surface contamination and gas delivery before attributing it to a particular cause. Establish repair and examination requirements from the inspection plan.
Contact-tip-to-work distance describes the distance from the contact tip to the work. Electrode extension is the length of unmelted wire beyond the contact tip. The arc occupies part of the tip-to-work distance, so use the term and measurement in the procedure.
Recognize a metal-cored setup
Metal-cored arc welding (MCAW) uses a continuous tubular electrode filled predominantly with metallic ingredients. Product formulations can contain deoxidizers and arc stabilizers. The external gas still provides shielding. Some wires are designed for high deposition and little residue. Glassy silica islands can occur, which can look different from the heavier slag layer of a flux-cored weld. Use the approved cleaning requirements for later passes or coating.
In a weld bay, compare the spool identification and gas with the approved WPDS. A product that can weld over light scale under some conditions still has to meet the project preparation requirements. A wire change can affect required settings and qualification. Lincoln Electric metal-cored product example.
What is an inspection concern if a shop substitutes short-circuit transfer for the specified pulsed spray on a structural groove weld?
The procedure change needs disposition and unsuitable settings can result in incomplete fusion.
Every short-circuit program uses pure argon.
Short-circuit transfer always requires a flat position.
The process becomes shielded metal arc welding.
A shop proposes switching a steel weld from globular to conventional axial spray transfer. What must the proposed setup account for?
DCEN and eliminating the gas supply.
A nonconsumable tungsten electrode.
A suitable shielding gas and current above the transition for the particular electrode and setup, covered by the applicable procedure.
Selecting vertical-down travel regardless of the procedure.
A gas-shielded metal-cored weld made beside an open bay door shows glassy islands and pinholes. What is the most supportable observation?
Both features can be accepted without evaluation.
These features prove granular submerged-arc flux was omitted.
The wind speed alone proves the weld conforms.
The glassy islands can be residues from the electrode. The pinholes warrant examination and checks of shielding and contamination.
Sections you finish are checked off in the contents.