5.3 Edge Preparation, Thermal Cutting Quality & Backgouging
Key Takeaways
Conventional oxy-fuel cutting uses oxidation and ejects the oxides. Plasma melts and ejects material and can cut conductive metals such as stainless steel and aluminium.
Air carbon-arc gouging uses a carbon electrode arc to melt metal and compressed air to remove it.
Check prepared edges for specified dimensions, surface condition and fit. Different material grades may need different thermal controls.
Backgouging exposes sound weld metal for the subsequent weld when specified. Inspect the profile, surface condition and any required evidence before it is covered.
Use the approved joint or repair procedure for preparation, cleaning, examination and the assigned release decision.
Compare the preparation methods
A prepared edge has two jobs. It must create the specified joint geometry and present an acceptable surface for welding. Check the material, process and the approved detail before accepting an edge. A smooth edge can have an incorrect bevel or root face. An accurately located bevel can still have a notch or contamination requiring attention.
| Method | How it removes material | What to inspect |
|---|---|---|
| Mechanical preparation | Milling, sawing or grinding forms the edge by mechanical removal | Compare the angle and land, inspect burrs and record any overheating or damage |
| Oxy-fuel cutting | A heated region of suitable steel oxidizes when exposed to the cutting oxygen stream. The jet ejects oxide from the cut. | Check cut angle, striations, notches and retained dross |
| Plasma arc cutting | A constricted jet of ionized gas melts material and ejects it | Look for taper, rounded top edges, dross and variation in the cut width |
| Air carbon-arc gouging | An arc between the carbon electrode and workpiece melts metal. Compressed air expels it from the gouge. | Check depth and access, look for residues and verify the required dressing before welding |
Conventional oxy-fuel cutting is suited to many carbon and low-alloy steels. It needs a reaction that can sustain the cut and oxide that can be removed. Refractory oxides make the conventional process unsuitable for typical stainless steel and aluminium cutting. Plasma removes metal by melting. It can be selected for electrically conductive alloys including stainless steel and aluminium. Select a process based on material, thickness, edge requirements and available equipment. TWI on oxy-fuel cutting and TWI on plasma arc cutting.
Verify cut-edge and fit-up condition
- Locate the surface. Identify the material grade and prepared side. Confirm the approved joint geometry and drawing revision. Check the bevel, root face and surface condition before the joint is tacked.
- Check cut quality. Record notches, rough gouges, dross and damage at identifiable locations. Variation in drag lines and edge squareness may indicate changes in cut quality. Appearance alone does not identify the cutting settings that caused the condition.
- Apply material and joint requirements. Thermal cutting creates a heat-affected edge. Some grades are sensitive to hardening, softening or delayed cracking. Review the specified process, temperature control and examination for that material. Grade-specific cutting guidance illustrates why one universal preheat or amount to grind cannot be applied to every plate. SSAB cutting guidance.
- Evaluate before covering. Use the governing acceptance criteria and procedure for rounding, dressing, re-cutting or repair where required. Recheck dimensions after approved dressing. An edge that looks cleaner can still fall outside the preparation tolerance if too much material was removed.
In a production choice between a machined bevel and a thermally cut one, compare access, tolerance, equipment and any required dressing or examination. A faster cut may require more work afterward. At a field joint, verify whether both sides remain accessible after erection before assigning inspection points. Follow the prescribed handling, PPE and hot-work process for the operation.
Worked check. A detail requires an edge free from pronounced gouges and a root face from 1.5 to 2.5 mm. One location has adherent dross and a 2.0 mm root face. The dimension fits, but the remaining surface condition needs resolution under the procedure. After approved dressing you measure 1.2 mm at that location. The root face is now 0.3 mm below the stated lower limit. Record both results, and avoid accepting the joint on the basis of its improved appearance.
Verify backgouging before second-side welding
Backgouging removes weld and base material from the reverse side to expose sound metal and create the opening specified for subsequent welding. It can be part of a two-sided CJP procedure. Air carbon-arc gouging and mechanical removal may be used where permitted. Follow the required profile, cleaning and inspection steps. A carbon-rich layer can form in some gouging conditions. The equipment or repair instructions and the governing procedure specify when and how to dress the surface. TWI on air carbon-arc gouging.
Check that the excavation reaches the intended region and that the specified welding process can access the root and sidewalls. Document remaining visible residue or a suspected discontinuity. Perform or arrange the examination specified by the inspection plan, which can include magnetic particle or penetrant testing where applicable. Record the method, scope and results. Each method has detection limits. Use the designated release process before the required evidence is covered by the next weld.
Why is conventional oxy-fuel cutting generally unsuitable for aluminium and austenitic stainless steel?
Stainless steel and aluminum have lower melting points than carbon steel, so the preheat flame vaporizes the kerf
The conventional process needs sustained oxidation with removable oxides. These materials form refractory oxides that hinder the cut.
Pure oxygen reacts explosively with stainless steel and aluminum at ambient temperature
Stainless steel and aluminum are non-conductive and cannot sustain the OFC electric arc
A procedure requires a clean backgouge that gives access to the root and meets the stated profile. Which observation calls for correction before release?
A clean profile that meets the stated geometry and examination requirements.
A completed examination report for the correct weld showing satisfactory results.
The required root access with the gouge dimensions within the specified range.
Adherent residue and a narrow excavation that falls outside the required profile.
For a procedure that specifies thermal edge preparation followed by two-sided welding with backgouging, put these checks in the documented order.
Arrange the items in the correct order
Complete the first side and excavate the second side as specified.
Confirm material, thermal cutting and preparation requirements.
Inspect the cut bevel and completed fit-up before welding.
Verify the prepared excavation and complete the examination specified for second-side release.