8.3 Welding Metallurgy, Carbon Equivalent & Material Traceability

Key Takeaways

  • In a fusion weld, the weld metal solidifies from liquid. The heat-affected zone is base metal whose structure or properties change due to welding heat.

  • Austenite in steel can transform on cooling. Composition and the thermal cycle influence which microstructures form.

  • Carbon equivalent helps assess steel hardenability and weldability under the specified method. Its value alone cannot prescribe a preheat temperature.

  • Match material reports, grades, conditions and heat or lot identifiers to the project and the actual pieces.

Last updated: November 2026

Read the thermal history of a fusion weld

The weld metal is the metal that melts and solidifies in making the weld. It includes melted base metal and any filler metal added. The fusion boundary separates weld metal from the adjacent base material. The heat-affected zone (HAZ) is base material next to the weld whose microstructure or properties changed from the heat. Farther away, the unaffected base metal retains its prior condition. The size and properties of these regions depend on the material and heating and cooling history. TWI on carbon and low-alloy steel weldability.

Steel microstructures and properties

Ferrite and austenite have body-centred cubic and face-centred cubic crystal structures, respectively. In a simplified iron–carbon phase diagram, which phases can exist at equilibrium depends on carbon content and temperature. A weld cycle is rapid and uneven, so the cooling path also matters. Some steel close to the fusion boundary may heat into the austenite range and then transform into different products:

TermHow to recognize the concept
FerriteAn iron-rich phase. In many low-carbon steels it provides a relatively soft, ductile matrix
PearliteAlternating layers of ferrite and iron carbide, often formed during sufficiently slow cooling
BainiteA family of transformation structures formed from austenite with ferritic regions and carbon redistribution
MartensiteA transformation product formed by shear without long-range diffusion. Untempered steel martensite can be hard and crack-sensitive

A susceptible steel can form a hard HAZ after fast cooling. Diffusible hydrogen, a susceptible microstructure and tensile stress can combine to produce hydrogen cracking. The actual risk depends on more than a phase name. Yield strength describes the onset of specified permanent deformation, tensile strength the maximum engineering stress in a tension test, ductility the capacity for plastic deformation, and notch toughness the resistance to fracture under specified notched test conditions. Hardness is resistance to indentation in the test used. One property does not establish the others. Cambridge steel microstructure research and TWI on steel HAZ hardness and toughness.

Identify the material family and condition

MaterialWhat the inspector looks for
Carbon and low-alloy steelsMaterial grade, thickness, restraint and specified hydrogen and thermal controls. The same steel can cool differently in a thin coupon and a heavy joint
High-strength low-alloy steelsVerify grade and production route. Some use microalloying and controlled processing. Use the applicable weldability method and check limits intended to preserve weld-area properties
Quenched and tempered steelsQuenching can create a hard structure. Subsequent tempering adjusts hardness and toughness. The specified welding heat cycle can matter for both hydrogen cracking and HAZ softening
Austenitic stainless steelsControl chemistry and welding practice for the application. Chromium carbide precipitation during an adverse time-temperature exposure can deplete chromium near grain boundaries and raise susceptibility to intergranular corrosion. Low-carbon grades reduce the risk
Aluminum alloysIn some heat-treated alloys, welding alters strengthening precipitates and can soften the HAZ. Check the alloy and temper, filler and specified oxide and contamination controls
Cast irons and nickel alloysIdentify the type before accepting a repair procedure. Some cast irons develop hard, crack-sensitive regions. Nickel-bearing fillers may be specified for cast iron. Some nickel alloy welds are susceptible to hot cracking if contaminants remain

Check the material and heat-treatment condition required by the drawing. A steel called out as quenched and tempered is supplied in a defined condition. A separate post-weld heat treatment, if specified, must follow the project procedure. TWI on quenched and tempered steel, Outokumpu on stainless steels, TWI on aluminum, cast iron and nickel alloys.

Hardfacing deposits a surface layer selected to resist wear. Dilution with base metal can change the deposited layer’s properties. Check the specified substrate and consumable, layer and finished thickness, and the surface acceptance criteria for that application. For example, the repair of a worn surface calls for a different verification plan from joining two structural members. TWI weld hardfacing research.

Calculate and interpret an IIW carbon equivalent

Use the calculation specified for the steel and application. The International Institute of Welding (IIW) carbon equivalent uses element contents entered as mass percent values:

CEIIW=C+Mn6+Cr+Mo+V5+Ni+Cu15.CE_{\mathrm{IIW}}=C+\frac{Mn}{6}+\frac{Cr+Mo+V}{5}+\frac{Ni+Cu}{15}.

An example report gives C 0.18, Mn 1.32, Cr 0.15, Mo 0.05, V 0.05, Ni 0.15 and Cu 0.15. The calculation is 0.18+0.22+0.05+0.02=0.470.18 + 0.22 + 0.05 + 0.02 = 0.47. If the purchase specification explicitly caps this calculated value at 0.45, flag the result as 0.02 above the stated limit. If the intent is to check preheat, use the applicable material, thickness, procedure and code rules. A higher value can signal increased hardenability for comparable steels. There is no universal preheat threshold applicable to every report or alloy. Missing chemistry is not zero unless the governing calculation permits that treatment. TWI review of carbon equivalent formulae.

Follow the report to the piece

Compare the drawing or bill of materials with the material test report (MTR) and the installed or issued piece. Check specification, grade, condition, applicable size, and the applicable chemistry and mechanical results. Check the traceable heat, lot or piece identifier under the project method. When stock is cut, verify that the method retains the link through fabrication. A loose MTR for a matching grade cannot establish which cut piece came from that heat. Document a broken link and refer it before the piece is accepted. ISO on steel inspection documents and ASTM example of structural steel marking.

Loading diagram...
Read the fusion weld cross-section from the centre outward
Test Your Knowledge

Using the IIW formula, what carbon equivalent results from C 0.21, Mn 1.26, Cr 0.10, Mo 0.10, V 0.05, Ni 0.15 and Cu 0.15 mass percent?

A

0.36

B

0.42

C

0.49

D

0.58

Test Your Knowledge

Which change explains sensitization of susceptible austenitic stainless steel after an adverse thermal exposure?

A

The steel loses all of its nickel from the weld region.

B

The oxide melts and turns the base metal into an aluminum alloy.

C

Grain boundaries acquire enough chromium to improve corrosion resistance.

D

Chromium-rich carbides precipitate at grain boundaries and deplete chromium nearby.

Test Your Knowledge
Ordering

Order the traceability checks from receiving requirements through fabrication.

Arrange the items in the correct order

1

Check the test report against the specified material information.

2

Confirm the link is retained as stock is cut and issued to fabrication.

3

Verify the issued stock identifier against the approved report.

4

Read the drawing and bill of materials for the specified grade and condition.

Sections you finish are checked off in the contents.