12.3 Cracks, Porosity, Inclusions & Incomplete Fusion: Causes & Detection (WFIC-301)

Key Takeaways

  • Crack orientation and location describe an indication. Timing can guide investigation without establishing its mechanism.

  • Porosity is trapped gas. An inclusion is trapped material such as slag or a metallic particle.

  • Incomplete fusion concerns an unfused interface. Incomplete joint penetration concerns the required depth at the root.

  • Inspect accessible stages as assigned and report hidden or unverified areas. Follow the project’s examination methods and timing.

Last updated: November 2026

Classify cracks and investigate their timing

A crack is a fracture that can initiate in weld metal or parent metal. Describe location, direction and extent as visible. A longitudinal indication follows the weld axis. A transverse one crosses it. A crack at a toe or root indicates a location. It does not identify its mechanism. Treat a suspected crack promptly through the inspection procedure and compare it with the applicable acceptance requirements.

Possible mechanismEvidence that can support investigation
Solidification crackingOccurs as weld metal solidifies. A centreline crack or a branching crack in the final crater can be associated with shrinkage and solidification conditions
Hydrogen cracking in susceptible steelsCan arise after cooling, including in the heat-affected zone or weld metal. Diffusible hydrogen, a susceptible microstructure and tensile stress contribute. Timing and location alone cannot prove the cause
Lamellar tearingCan develop in susceptible rolled parent plate when welding strains act through its thickness. Investigate the material, joint geometry and restraint

Use the delay, if required, in the governing work instruction or code. A clear initial visual examination cannot rule out a discontinuity that appears later. For example, report a new toe indication identified during an assigned re-examination. Record both inspection times and the area examined. Preserve the material, consumable and thermal records for the responsible reviewer. TWI on solidification cracking, hydrogen cracking and TWI on lamellar tearing.

Separate trapped gas and trapped material

Porosity is gas trapped in the weld as it solidifies. Some pores are isolated or scattered. A reported pattern may be clustered, aligned or elongated. Shielding, contamination and welding conditions can contribute. At a visible surface, record the size, count or extent and grouping as the applicable rule requires. Paint damage, dirt or other marks can resemble openings. Confirm the evidence before assigning a type. Valid pore diameter comparisons and lengths depend on the tool and procedure. TWI on porosity.

An inclusion is solid material trapped in the weld. Slag can be trapped at an interpass toe when the profile obstructs cleaning or during deposition. A tungsten particle can enter the deposit if a gas tungsten arc welding electrode contacts the pool or becomes damaged. Check the stated interpass cleaning before additional metal hides the surface. A radiograph may display a dense inclusion differently from a void. A qualified examiner interprets it under the procedure. Visual evidence alone cannot characterize buried material. TWI on slag inclusions and CWB on radiography.

Locate the unfused interface or unfilled root

Incomplete fusion describes a failure to fuse where fusion is required, such as at the groove sidewall, between weld passes or at a root face. An exposed unfused sidewall may be visible during deposition. Record where it is and which pass it is beside. Heat, angle, access, heavy oxides or technique may be involved. A cap on top cannot demonstrate that the sidewall below it fused.

Incomplete joint penetration concerns the penetration required at the root of a groove weld. An accessible root with an unfilled original joint line may indicate that the required depth was not reached. Confirm the stated joint design. In a partial-joint-penetration weld some depth is intentionally left unwelded. For the prescribed criteria check the accessible surfaces and the required method. TWI on incomplete sidewall and inter-run fusion and TWI on root fusion and penetration.

Worked staged examination

A procedure and inspection plan require checking the accessible root before depositing fill, then checking cleaned surfaces between passes at assigned stages, and finally examining the completed surface. During the first assigned fill-stage check, an exposed sidewall appears unfused beside the pass. Record the weld ID, side and length. Notify the supervisor and keep the stage accessible for disposition as required. Even if the accessible root appears sound, the sidewall indication still needs assessment. Any buried condition must be evaluated by a suitable authorized examination. Reflect inspection limitations in the report.

In a second example, three pinhole indications are visible on a cleaned face after an unexpected change in shielding. Identify the location of each opening, size it by the designated method and check the applicable pattern criterion. Report the recorded gas change separately. A surface opening can support an investigation of porosity, but it cannot prove that the underlying weld is porous throughout or that the gas change caused it.

Loading diagram...
Match the indication to the accessible stage
Test Your Knowledge

Which combination can contribute to delayed hydrogen cracking in a susceptible steel weld or heat-affected zone?

A

High helium flow, low sulfur and high voltage.

B

Tungsten contact, zero restraint and surface porosity.

C

Diffusible hydrogen, a susceptible microstructure and tensile stress.

D

Long weld length, a clean nozzle and low carbon on their own.

Test Your Knowledge
Ordering

Order the stages in the stated multipass inspection plan.

Arrange the items in the correct order

1

Check the cleaned surfaces between passes at the assigned stages.

2

Examine the exposed root before it is covered.

3

Examine the finished surfaces under the specified conditions.

4

Verify pre-weld preparation and fit-up.

Test Your Knowledge

During an assigned fill-stage inspection, the original groove sidewall is visibly unfused beside the new pass. What should the inspector report?

A

An apparent incomplete sidewall fusion at that area, with its location and extent.

B

An incomplete root penetration finding solely from the sidewall.

C

A proven hydrogen crack in the base metal.

D

An acceptable weld because the visible root looks sound.

Sections you finish are checked off in the contents.