11.1 Filler Metal Classifications (AWS / CSA W48, Tungsten & SAW Fluxes)
Key Takeaways
CSA W48:23 refers to AWS or ISO standards for testing and classification and retains consumable certification requirements.
Decode a designation under the applicable specification. Similar strength labels do not establish an approved substitution.
Check the exact wire, applicable shielding gas, polarity and position or technique requirements.
For submerged arc welding, verify the specified electrode and flux combination. Tungsten has a separate electrode classification.
Read the classification in context
First identify the process, material family and standard on the procedure. CSA W48:23 retains Canadian welding consumable certification provisions and references AWS or ISO standards for classification and testing. CWB explains that the 2023 edition moved classification and testing out of the standard’s own tables. Some older labels or certificates use earlier designations. A shop may have both metric and US customary designations for the same product. Check the governing specification and actual evidence. When certification is required, the CWB directory identifies supported product entries with fields such as manufacturer, trade name, class, diameter, applicable gas or flux and place of manufacture. CWB on W48:23 changes and CWB certified welding consumables.
Decode a covered steel electrode
In the AWS A5.1 example E7018, E identifies an electrode, 70 refers to 70 ksi minimum tensile strength for specified deposited-metal test conditions, 1 designates all-position classification, and the last digit is read with the position digit to identify covering and usable current. E7018 is a low-hydrogen iron-powder class used with the conditions identified by the product and procedure. E7024 is a different iron-powder titania class for flat and horizontal fillet use as classified. The shared 70 strength designation does not make them interchangeable. The class describes test and usability criteria, so check the actual position, diameter and polarity permitted for the weld.
In examples such as E7018-1 H4R, -1 identifies additional impact requirements under the applicable classification, H4 identifies a maximum of 4 mL diffusible hydrogen per 100 g of deposited weld metal in the specified classification test, and R designates a moisture-resistance requirement for the covering. It does not waive handling limits. For example, Lincoln’s Excalibur 7018-1 MR lists AWS E7018-1 H4R and a CWB designation E4918-1-H4R. They are published designations for that product. The unit conversion of 70 ksi is approximately 483 MPa and cannot by itself assign a product to a metric class. AWS A5.1/A5.1M:2026 scope, Lincoln on electrode classification and dual-listed product example.
Identify wires, rods and cored electrodes
| Process or material | Example and its inspection meaning |
|---|---|
| Solid carbon-steel wire | ER70S-6 is a solid carbon-steel electrode or rod class. The suffix identifies a composition class. Manganese and silicon can aid deoxidation. Use the required joint preparation and gas |
| Gas-shielded flux-cored wire | A product can have distinct gas-based classifications. For example, Lincoln Outershield 71M lists C and M designations with test information for carbon dioxide and argon–carbon dioxide. Read the process and wire listing with the actual gas |
| Self-shielded flux-cored wire | Verify the listed product and its intended shielding and polarity. Do not supply external gas just because the wire is tubular |
| Stainless, aluminum and nickel | AWS A5.9, A5.10 and A5.14 cover examples of bare electrode or rod classifications for these families. Read the alloy designator and application under the applicable specification. The carbon steel strength-digit example cannot decode alloy designations |
Do not approve a switch because two wires have similar descriptions. For a cored wire, the usability classification and gas or test designator can have different meanings across fixed or open classification systems and editions. Compare the product label and the approved setup using the specified standard. AWS A5.18/A5.18M:2025, AWS metal and process specification index, Lincoln ER70S-6 example and gassed cored wire example.
Check tungsten and the submerged arc pair
Gas tungsten arc welding uses a nonconsumable tungsten electrode. The classification identifies composition or additions, and the applicable specification supplies an identification marking. Match the package and markings to the electrode required by the procedure. Thoriated tungsten contains radioactive material. Grinding can generate dust, so use the applicable hazard and shop controls. AWS A5.12M/A5.12:2024 and AWS review of tungsten electrode exposure.
For submerged arc welding (SAW), identify both the electrode and the flux. The pair’s classification can depend on test condition and mechanical results. A manufacturer’s example of F7A2-EM12K-H4 identifies EM12K wire with a particular flux and as-welded classification results. Active flux can influence manganese and silicon transfer as welding parameters change. Use only the specified combination and technique, including any pass restrictions. If a flux was changed mid-weld, record the actual products and affected passes before seeking disposition. AWS A5.17/A5.17M:2025, Lincoln SAW combination example and TWI on active and neutral fluxes.
The procedure specifies E7018 for a vertical steel weld. The store issues E7024. What does the classification check show?
Both classes use the same covering and position because they start with 70.
E7024 is an aluminum electrode for the stated position.
The two classes differ in covering and position capability. A shared strength designation does not authorize the substitution.
E7024 may be substituted automatically if its packaging is sealed.
Under its applicable classification, what information does H4R add to a covered electrode designation?
A hydrogen limit under the classification test and a covering moisture-resistance designation.
A specified four-hour oven temperature and a red marking.
A four percent alloy addition and unrestricted exposure.
Four required uphill passes and a restriction to reverse travel.
An SAW wire matches its label, but the flux was changed to a product outside the approved wire–flux combination. What should the inspector record?
No deviation if the flux is the same color.
No deviation if the wire size remains unchanged.
Only the voltage displayed on the source.
The unapproved flux, wire, applicable procedure and affected joints or passes for disposition.
Sections you finish are checked off in the contents.