12.4 Special Piping

Key Takeaways

  • A flare seals on a formed cone. A compression fitting uses the specified ferrule or ferrule set and its own makeup procedure.

  • Filler-metal liquidus separates soldering from brazing. Joint design, material condition and the governing code determine service suitability.

  • Check finished bend radius, plane, ovality and wall thickness against the applicable design. A bend can pass one check and fail another.

  • Protect glass lining from impact, flange distortion and thermal shock. Use the specified gasket, bolt-loading procedure and inspection criteria.

  • A hydraulic ferrule preset still requires final fitting-body assembly. Lokring, seal-element press fittings, and grooved couplings each use their own tool and acceptance checks.

Last updated: November 2026

Special Piping

Quick Answer: Module 08406 covers flared and compression joints, soldering and brazing, pipe bending, glass-lined piping, and mechanical tubing joints. The current module specifically includes Lokring and crimped connections. This section also covers ferrule preswaging and grooved system management. Identify the actual joint first. The joining procedure establishes the tooling, fit-up, inspection and service limits.

Copper tubing: flared joints

Flared joints form a cone on the tube end that seals against a fitting seat under a flare nut.

Typical process:

  1. Cut the tube square, ream the bore and deburr the outside edge as the fitting instructions require.
  2. Slide the matching flare nut onto the tube in the correct direction before forming the cone.
  3. Clamp the tube in the flaring block with the correct projection beyond the die face
  4. For a specified SAE 45° connection, form the cone with a compatible 45° tool sized for the tubing. Other flare systems can use a different angle.
  5. Inspect for cracks, uneven skirts, and over-thin edges; recut if defective
  6. Seat the flare on the mating cone, then tighten to the fitting manufacturer’s requirements.
Flare defectCause / result
Split flareCheck for burrs, incorrect tooling or tubing temper outside the specified range.
Off-center flareTube not square or not seated in block
Nut omitted before flaringIf the remaining length permits, cut off the flare and form a new end with the nut in place.
Under-flareLeaks under pressure

Use the tubing specified for the joint. The Copper Development Association recommends annealed Types K or L for flaring. If the specified method permits local annealing of rigid tubing, follow the approved procedure and associated hot-work controls.

Copper tubing: compression joints

A compression fitting uses one ferrule or a ferrule set. Nut movement drives the ferrule assembly against the fitting body and tube to grip and seal it. Confirm tube outside diameter, wall and material, and use the matched fitting components.

  • Square-cut and deburr the tube, then push it to the shoulder or approved depth.
  • Follow the product's specified starting position, wrench turns or torque, and inspection. For example, the Swagelok MS-12-01 procedure for typical new ½-inch two-ferrule joints tightened by the standard manual method uses 1¼ turns from finger-tight with the body held steady. Check the initial makeup with the specified gauge. Small sizes and special service have their own requirements.
  • Follow the manufacturer's instructions for any remake, including limits on ferrule and body compatibility. Swagelok's initial-installation gap gauge is used on new makeup and is excluded by its reassembly instructions.
  • Support the tube and look for scratches, poor insertion, damaged parts or an incorrect makeup procedure if a connection leaks. Verify isolation before correcting it.

Brazing vs soldering

For the copper tube socket joints here, molten filler moves through the fitted clearance by capillary action while the components remain solid. The process distinction is the filler’s liquidus, the temperature above which it is fully liquid. Brazing uses filler whose liquidus is above 450°C (about 840°F), below the base material's solidus. Soldering uses filler at or below the boundary. Verify the filler and joint design for service.

Selection factorSolderingBrazing
FillerSpecified solder. Use lead-free products where required for drinking water.Specified brazing filler, such as an approved copper–phosphorus alloy for copper to copper.
PreparationClean mating surfaces and apply the specified soldering flux.Clean mating surfaces. Choose the flux or atmosphere for the filler, base metals and process. Copper–phosphorus filler can be self-fluxing on copper to copper.
Process piping under B31.3-2024§317.1 limits soldered joints to Category D Fluid Service and requires §333.§317.2 permits brazed joints made to §333 in Normal Fluid Service, requires safeguarding in services that are flammable, toxic or damaging to human tissue and excludes severe cyclic conditions.
Heat and performanceFollow the specified joint design and protect adjacent parts from heat.Higher temperatures can anneal hard copper tube near the joint. Evaluate the assembled joint using the applicable rating and material condition.

For covered B31.3 work, follow §333 for personnel, procedures and materials. For Category D brazing at a design temperature no higher than 200°F, §333.1.1 allows an exception to brazing qualification unless the engineering design requires it. Solderer qualification follows ASTM B828 under §333.1.2. Building plumbing and refrigeration may use different governing codes and approved procedures.

Craft sequence. Verify the correct tube, fitting and clearance. Clean the joint surfaces, apply flux where required and assemble to the specified depth. Support the parts so they stay in position. Under the applicable hot-work controls, heat the assembly as prescribed and feed filler at the joint so it enters the clearance. Follow the procedure for cooling, cleaning residual flux and examination. Use the specified inert purge where required, such as in some refrigeration procedures, with a safe discharge path.

Pipe bending

Start with the specified centerline radius, bend angle, plane and tangent lengths. Select a bender and tooling approved for the actual outside diameter, wall and material. Hand lever benders suit specified small tubing, while larger jobs can use powered or engineered induction equipment. Use the tool's take-up and position marks. For example, the developed centerline arc of a 90° bend with a 6 in. centerline radius is 6 × π ÷ 2 ≈ 9.42 in. Tangents and tooling allowances are separate. Verify the finished angle after unloading since the pipe can spring back.

Under ASME B31.3-2024 §§332.1–.2, finished bends must be free of cracks, substantially free of buckling, and at least as thick as the design requires. Measure maximum and minimum outside diameters in the same plane perpendicular to the bend’s centerline. Under the ordinary §332.2.1 criterion, their difference can be no more than 8% of nominal OD for internal pressure and 3% for external pressure. Apply any tighter project limit. An alternate pressure-design qualification for a bend outside the code ovality limit requires engineering review under §§306.2.1(b) and 304.7.2. Grinding away metal to meet the ovality limit is prohibited.

For a 4.500 in. nominal OD pipe with 4.55 in. maximum and 4.30 in. minimum readings at one bend cross section, ovality is (4.55 − 4.30) ÷ 4.500 × 100 ≈ 5.56%. That meets the ordinary internal-pressure ovality limit but exceeds the external-pressure limit. It establishes no result for remaining wall thickness or other cross sections.

Bend checkWhat to verify
Tooling and workpiece supportCorrect die, and mandrel or other support when specified, to prevent collapse and control shape.
Radius, legs and planesFinished dimensions and rotation against the approved drawing, including compound bends.
Wall thickness and shapeCheck the outside of the bend where thinning can occur, and examine the inside for buckling.
Heating or cold formingUse the approved procedure, material/temperature limits and specified heat treatment.

Glass-lined piping care

Glass-lined steel uses a steel shell and a glass corrosion barrier. A blow, local bending load or sudden temperature change can damage the lining even when the shell still looks sound.

  1. Before removal, establish the specified isolation, drain the line and verify conditions for opening. Support the spool before releasing bolts. Keep end covers on removed and replacement spools during handling. Use approved lift points and slings that protect the pipe and faces. Keep hard tools off the glass.
  2. Check the lining and flange faces for defects before closing the joint. Use the prescribed inspection procedure and report damage. Follow the specified electrical inspection settings where applicable.
  3. Support and align the spools within the procedure. Install the approved gasket, then apply the manufacturer’s bolt-load sequence and limits. De Dietrich's glass-lined piping catalog distinguishes torque values by flange and gasket construction.
  4. Follow the specified temperature-change limits during operation. Leave lining repair or replacement to the approved repair process.
ObservationAction
Chipped flange or star-shaped crackProtect the area and obtain the specified inspection and disposition.
Faces fail alignment limitsResolve the support or fit-up problem before tightening.
Dissimilar gasket proposedConfirm compatibility and seating load with the project and product instructions.
Adjacent welding or grinding proposedProtect or remove the lined component per the approved method before work.

Hydraulic compression and press joints

In a hydraulically preset ferrule system, the tool forms the ferrule assembly on the tubing before final fitting-body assembly. For example, on the Swagelok Multihead Hydraulic Swaging Unit, select the die, tube and ferrule set the instructions specify. Prepare and seat the tube in the die with the nut and ferrules correctly oriented. Stop pumping when the indicator releases. Open the bypass as instructed, remove the assembly and check the tube end for the required bottoming mark. Assemble the accepted preset tube into the fitting body, apply the specified final nut makeup and verify it with the correct MHSU gauge. Incorrect tooling, an incomplete stroke or the wrong final makeup can leave the joint unfit for service.

A Lokring elastic-strain-preload fitting uses a hydraulic tool to move a driver ring axially over the fitting body. That swages the body onto the pipe or tube to make a metal-to-metal seal. Prepare the outside surface as specified, make the required installation and inspection marks, and insert to the required depth. Use the correct tool and check the final marks and driver position against Lokring LP-105.

A seal-element press fitting uses a matched jaw or ring to form the fitting onto the tube or pipe. For example, Viega MegaPress calls for a prepared and deburred pipe, an intact seal and other required components, marked insertion depth, a full press cycle with the prescribed tool, and inspection. Confirm the exact fitting's application and test limits and use the approved leak-test procedure. Account for press-tool pinch points and isolate the process before modifying piping.

Grooved piping systems management

Beyond initial assembly (covered with Module 08306 skills), managing grooved systems means keeping them reliable through startup and operations:

  1. Verify coupling style (flexible vs rigid) matches the design intent for movement and alignment
  2. Maintain support spacing so couplings are not overloaded in shear or hanging weight improperly
  3. Inspect for visible corrosion, damage, or leakage. Use the coupling model’s assembly and inspection criteria for key engagement, bolt pads and fasteners. Follow the approved isolation procedure before adjustment or disassembly.
  4. Set the end gap for the selected flexible coupling and the designed direction of movement. An excessive gap can leave the gasket or keys outside their intended engagement.
  5. For any modification, prepare ends to the specified groove profile for that pipe and coupling, and gauge the result before assembly.
  6. Isolate, depressurize, drain and verify conditions before removing housings. Follow the manufacturer’s disassembly procedure.
  7. Keep the exact approved gasket grade for the fluid, temperature and chosen housing. Follow the model’s reassembly instructions.
Management taskWhy
Periodic visual on large racksDetect visible damage, corrosion, leaks or a change in joint position.
Document flexible coupling locationsThermal growth strategy depends on them
Train crews not to use couplings as permanent anchorsLoad path was not designed that way

Scenario: solder where braze was specified

A refrigeration job specifies a brazed copper socket joint. The installer discovers that one joint was soft-soldered before pressure testing. Stop work and have the responsible team identify the extent of the substitution. If the line has been energized or charged, have authorized workers establish the required isolation and recover its contents under the approved procedure. Replace the joint using the specified filler and brazing procedure, including purge where specified, then complete examination and the applicable system test. A leak check would only show whether the joint leaked under that check's conditions.

Putting Module 08406 together

  1. Flare with the nut on first, square cuts, and inspect the cone; compress with full insertion and controlled makeup.
  2. Distinguish soldering from brazing by filler liquidus. Verify the joint and service requirements.
  3. Check radius, ovality, wall thickness, and finished surface on bends.
  4. Treat glass-lined pipe as impact- and distortion-sensitive.
  5. Use the correct tools and acceptance checks for ferrule, press and grooved connections.

Verify the completed joint and the required leak test before returning the piping to service.

Test Your Knowledge

Which property distinguishes brazing filler from solder in these capillary copper tube joints?

A

The brazing filler has a liquidus above 450°C and below the base material’s solidus.

B

The brazing filler must melt the base copper to fill the joint.

C

The solder must have a liquidus above 450°C if used with flux.

D

Any filler with a low melting point is brazing filler if installed with a flame.

Test Your Knowledge

A crew prepared a 45° flare, but the approved connection is a two-ferrule compression fitting. How should the crew prepare the tube for that fitting?

A

Use the flare as the front ferrule, then tighten the nut.

B

Prepare a square, deburred unflared end of the specified tube, fully insert it, and assemble the matched ferrules as directed.

C

Use the flare nut with the compression fitting if the threads engage.

D

Flatten the flared end with the compression nut during makeup.

Test Your Knowledge

A replacement glass-lined spool is ready for bolt-up. Which plan protects the lining at the joint?

A

Tighten the nearest bolt first to pull an offset nozzle into position.

B

Dress the glass surface with an abrasive to make a ring gasket seat.

C

Align and support the spool, use the specified gasket, and follow the approved bolt-loading procedure.

D

Increase the torque above the manufacturer’s limit to compensate for a thicker gasket.

Test Your Knowledge

The gap at a flexible grooved coupling is outside the specified range. What must be resolved before pressure is applied?

A

Only the outside paint color needs to be restored.

B

The gap can stay as found if the two pipes have the same nominal size.

C

The allowed gap may be exceeded whenever the bolt pads meet.

D

Verify and correct the gap so the gasket and keys seat and the joint retains the designed motion allowance.