10.2 Stress Relieving & Aligning
Key Takeaways
Check assembly-induced strain and the calculated equipment loads at the applicable cold, operating and test conditions.
Thermal expansion and contraction can load nozzles if the pipe cannot move as designed. Check pipe supports and clearances before fitting the spool.
Determine preheat and postweld heat treatment from the applicable code, engineering design and approved welding and heating procedures.
Check pipe flange fit and pump-to-driver alignment separately, then confirm that connecting the pipe did not shift the equipment beyond its limits.
Cold spring introduces a specified initial displacement and reaction. ASME B31.3 permits consideration for reaction calculations and gives no credit against the displacement stress range.
Stress Relieving & Aligning
Quick Answer: Module 08403 covers stress relief, thermal expansion, metal behavior and fit-up at rotating equipment. Use the approved support and alignment procedure to avoid harmful nozzle loads. Apply designed cold spring only as specified. When heat treatment is required, follow the controlled cycle rather than using it to close a fit-up gap.
Hangers hold weight; this section covers how the line is fitted, stressed, and aligned relative to equipment and temperature. Check how the pipe fits at installation and how the supports and equipment carry load after startup.
Residual stress and assembly strain
Uneven heating and cooling during welding can leave residual stresses. These stresses can contribute to cracking or distortion, depending on the material and service. A specified postweld heat treatment (PWHT) can reduce residual stress or achieve required metallurgical properties.
Assembly strain can arise when a spool is forced into position or a support transfers weight to a nozzle. Correct the fabrication, fit-up and support at the source. Use the applicable allowable nozzle loads and check conditions at installation and in service.
Key Point: Flange face alignment and bolt-hole alignment are separate checks. ASME B31.3-2024 §335.1 prohibits distortion during joint alignment when it introduces detrimental strain. Apply the specified flange tolerances as well as equipment limits.
Thermal expansion in piping
Metals expand when heated and contract when cooled. A long steel run that is cold during installation will grow when placed in hot service. If restraints prevent free growth, compressive loads can develop. A system can carry those loads or transfer them to supports and equipment, depending on its actual flexibility and restraint.
Practical implications for fitters:
| Condition | Expansion concern |
|---|---|
| Steam and hot process lines | Evaluate growth and use the flexibility, restraints and supports from the design. |
| Cryogenic / cold lines | Contraction when cooled; supports and anchors must allow designed shrink |
| Outdoor lines | Ambient swings plus sun load on dark pipe |
| Lines tied to turbines/pumps | Verify allowed forces and moments for the specific equipment. |
Set supports, guides and anchors where specified so the piping accommodates the calculated travel.
Temperature and metal structure (awareness)
Temperature does more than change length:
- Elevated temperature can reduce strength and increase creep risk in some alloys under long-term load
- Welding heat creates a heat-affected zone and residual stress. Preheat can slow cooling and reduce hydrogen-cracking risk. PWHT can temper susceptible microstructures or reduce residual stresses under the specified cycle.
- Thermal gradients (hot top, cold bottom, or partial fill) bend pipe and add stress even without full average temperature change
- Brittle fracture risk rises in some carbon steels at low temperature if toughness is inadequate—material selection and impact testing are engineering controls, but fitters must not ignore low-temp service warnings on procedures
Apply heat treatment when the governing code, material, control thickness and engineering design require it. Follow the approved WPS and heat-treatment instructions. For example, B31.3-2024 §331 controls the required cycle and its verification, including applicable heating and cooling limits and local heating.
- Follow the specified metal temperature, hold time, heat-up and cooling limits and temperature measurement method.
- Support the assembly so it does not sag under its own weight at heat
- Do not substitute torch “heating until red” for controlled PWHT when the code/job requires documented heat treatment
- Protect nearby instruments, equipment and spring supports from the heat. Keep the specified records.
Aligning pipe to rotating equipment
Pumps, compressors, turbines, and blowers have tight allowable nozzle loads and alignment tolerances. Distinguish base fit, shaft alignment and pipe fit. Soft foot is a poor fit between a machine foot and its mounting surface. Tightening that foot can distort the machine even before any pipe is attached. Pipe strain can impose an additional load after bolt-up.
Alignment principles for pipefitters
- Set the equipment and establish its initial alignment using the approved installation sequence. Fit the pipe to the set equipment, then compare its alignment before and after connection.
- Verify the flange clearance, parallelism and bolt-hole alignment before assembly. Resolve mismatches by correcting supports or the spool rather than drawing it up against the nozzle.
- Parallelism, centerline and elevation each matter. Misalignment can concentrate gasket load and distort the attached casing.
- Temporary supports may hold a spool during fit-up; permanent hangers must take the load before you claim alignment is done.
- Measure unloaded flange fit using the specified dimensional method. Compare shaft or casing readings before and after connecting the pipe using the approved indicator or laser procedure. Correct pipe strain when the readings exceed equipment limits.
| Bad practice | Why it fails |
|---|---|
| Using the pump nozzle to lift or swing a spool into place | Overloads casing and bearings |
| Drawing flanges together with long bolts and extreme torque | Stores elastic bend in pipe and equipment |
| Leaving a loaded chain fall attached to hold the spool against the nozzle after startup | Unintended load on the equipment |
| Shimming only one side of a flange to kill a gap | Creates permanent moment on the nozzle |
| Ignoring spring hanger cold settings near equipment | Incorrect spring force can shift load to the nozzle |
Exam Tip: If a stem asks how to correct a pipe that does not meet a pump flange, the answer is almost never “tighten until it comes together.” Correct the pipe spool, supports, or base—protect the nozzle.
Coordinating with millwrights and mechanics
Coordinate the pump-to-driver checks with the mechanic responsible for the equipment. For example, the ITT Goulds LF 3196 i-FRAME IOM calls for cold checks before grouting, after grouting and after piping connection, then a final hot alignment check after the first run at operating temperature. Use the limits for the actual cold or operating-temperature condition. Verify safe access and isolation per the IOM and site procedure before any adjustment. If connecting the pipe changes the reading beyond the permitted value, correct the piping and repeat the check.
Engineered cold spring
Cold spring is an intentional displacement applied during assembly to create a specified initial reaction. It can balance reactions at installation and at extreme displacement conditions. ASME B31.3-2024 §319.2.4 gives no credit for cold spring in displacement stress-range calculations. The designer can account for it under the code’s reaction calculations.
Before applying cold spring, verify the guides, supports and anchors can produce the intended motion. Under §335.1(b), check the preassembly gap or overlap against the drawing and correct discrepancies. Use the specified temperature conditions, datums, direction, closure method and records. Heating to close the gap defeats the cold-spring design and is prohibited by that provision. Resolve an unplanned misfit through the fit-up process.
Avoiding strain on equipment nozzles
Allowable nozzle loads are often small compared with the force a long pipe run can generate. Protect equipment by:
- Anchoring and guiding the pipe so expansion is directed into loops/joints away from the machine
- Supporting adjacent pipe so deadweight does not hang on the nozzle
- Using flexible elements (expansion joints, flexible hose where allowed, spring supports) only as designed
- Fitting spools within the equipment and assembly limits
- Checking after hydrotest and after insulation—weight and temperature changes move loads
- Transferring loads from temporary supports and releasing construction restraints in the planned sequence
Red flags during walkdowns:
- Hanger rods slack next to a pump while the nozzle looks loaded
- Spring cans still pinned beside a turbine inlet
- Large eccentric reducers hard against a compressor flange with no support under the valve weight
- Pipe resting on the equipment lifting lug or base instead of on its hanger
Stress control during fabrication and erection
Everyday practices that reduce locked-in stress:
- Follow fit-up tolerances for hi-lo and alignment before welding
- Use strongbacks and proper clamping—not extreme force that elastic-springs back after release
- Sequence welds to limit distortion when the WPS/site practice requires it
- Support cantilevered spools during welding so the joint is not stressed by its own weight
- After cutting out a bad fit, re-measure—do not stack correction upon correction until the last joint absorbs all error at the equipment
Scenario: ⅜-inch gap at a pump suction
A suction spool is ⅜ in. short of its specified fit and 1° out of parallel to the pump flange. The measurements are outside the approved fit limits. Keep the pump isolated and correct the spool or supports. Before reconnecting, repeat the gap, parallelism and shaft readings. After tightening with the approved gasket and procedure, compare the equipment readings to the unconnected baseline. This distinguishes a corrected flange fit from a remaining equipment alignment problem.
Scenario: specified cold pull on a steam line
The installation drawing calls for a 1-in. preassembly cold-pull gap at a designated joint and temperature. Once the permanent anchors and support settings are verified, the crew measures ¾ in. at the specified datum. The gap is ¼ in. short of the drawing value. Correct or obtain disposition of the discrepancy before closing the joint with the specified method. The gap is measured before applying the pull.
Putting Module 08403 together
- Distinguish heat treatment for residual stresses or metallurgical properties from correcting assembly strain.
- Plan for thermal expansion—temperature changes length and load paths.
- Align pipe to rotating equipment without using nozzles as jacks.
- Apply cold spring only when engineered and specified.
- Verify that supports carry their design loads and that equipment nozzle forces and moments remain within the approved limits.
Section 10.3 expands the expansion hardware and insulation systems that work with these alignment principles in service.
A pump suction connection is ½ in. short of the required fit and out of parallel beyond the approved limits. What should the crew do?
Draw the flanges together with come-alongs and extra-long bolts until the gasket seats
Use the pump casing as a jack by lifting on the nozzle with a chain fall until the faces meet
Leave a permanent come-along hooked after startup to hold alignment
Correct the spool and supports, then verify flange fit and the resulting equipment alignment
What is the purpose of a specified cold spring in piping assembly?
To introduce a calculated initial displacement and reaction so reactions can be managed across operating conditions
Any field habit of bending pipe by hand until it looks straight
The practice of removing all hangers so the pipe can expand freely in every direction
A requirement to hydrotest every line at ambient temperature only
Why can thermal expansion of a long hot pipe run damage a compressor or pump if supports are wrong?
Because hot pipe always loses all weight so hangers become unnecessary
Because expansion can generate large forces that transfer into equipment nozzles when movement is not directed into loops, joints, or guided paths
Because thermal growth only occurs in plastic pipe, never in steel
Because expansion reduces pressure to zero and collapses the casing
The governing requirements and approved welding instructions call for PWHT. Which practice is appropriate?
Heat randomly with a torch until the weld is dull red, with no temperature control or records
Skip heat treatment if the joint passed visual inspection only
Follow the specified temperature, hold time, heating/cooling rates, and support the assembly against sagging at heat
Cool the weld as fast as possible with water to lock in maximum residual stress
Sections you finish are checked off in the contents.