14.3 Glass Ionomers, RMGI, Dental Amalgam Alloys & Calcium Silicate Liners
Key Takeaways
Conventional glass ionomer sets by an acid–base reaction. Resin-modified glass ionomer adds a resin cure and still requires contamination control.
Select glass ionomer conditioning, surface protection and load-bearing indications from the product instructions.
High-copper amalgams form copper–tin reaction products, which reduce gamma-2 in many formulations. Creep and strength vary with alloy and handling.
Distinguish a liner over remaining dentin from a material placed directly on exposed pulp. A liner is unnecessary as a routine step under the current deep-caries guideline.
DHA directs contact and noncontact amalgam waste into airtight biohazard-labeled containers for the designated waste-management route.
Before choosing a material, determine whether the case calls for a definitive restoration, a liner or base beneath a restoration, or treatment of exposed pulp. Each use has different isolation and placement requirements.
Conventional and resin-modified glass ionomers
Conventional glass ionomer cement (GIC) uses an ion-leachable glass and an aqueous polyacid. The acid attacks the glass and releases ions that crosslink the polyacid in an acid–base reaction. The material can interact chemically with tooth mineral through calcium and carboxylate groups. It releases fluoride. Some formulations take up and release fluoride again after exposure, with differences among products. During early setting protect the material from contamination and dehydration as directed. A conditioner or protective coating can be part of the product-specific instructions. Original glass ionomer report · Primary fluoride release and recharge experiment · Fuji IX GP Extra capsule instructions
Resin-modified glass ionomer (RMGI) combines an acid–base reaction with resin polymerization. In a light-cured product the light fixes the initial form. Some formulations bond chemically to tooth mineral and release fluoride. Use isolation, conditioning, application and light settings from the specific product. For a cervical or root restoration, an indicated RMGI can be reasonable if the clinician can expose the margin and control bleeding and moisture. Fluoride release does not take the place of disease control. Primary setting study · Primary tooth interface study · Fuji II LC instructions
In a sandwich restoration, a compatible glass ionomer serves as a base under resin composite. A closed sandwich covers it with composite at the external margins. In an open sandwich, some base remains exposed at a margin, so the product must be suitable for that exposure. Choose the material for the site and load, following the restorative and base instructions. Fuji II LC restorative and base indications · Vitrebond Plus liner and base instructions
Amalgam composition and handling of waste
Dental amalgam sets by reaction of mercury with a silver–tin alloy containing copper. Older low-copper alloys can form a tin–mercury gamma-2 phase in addition to the silver–mercury gamma-1 matrix and remaining alloy particles. Gamma-2 is susceptible to corrosion and contributes to poor marginal behavior. In many high-copper alloys, tin reacts with copper to form the eta-prime phase (), reducing or eliminating detectable gamma-2. Creep is time-dependent deformation under load. Alloy composition and handling influence creep and marginal properties, so phase chemistry alone cannot predict the life of an individual restoration. Original amalgam microstructure study · Primary high-copper analysis · Primary creep study · Clinical marginal fracture data
When removal is clinically indicated, water spray and high-volume evacuation help reduce exposure while cutting amalgam. For contact and noncontact amalgam waste, Dubai Health Authority (DHA) CG-10 issue 2 specifies airtight containers labeled as biohazard waste and disposal through the waste-management unit under local regulation. Keep amalgam waste out of the ordinary waste stream and drains. The guideline also advises against heat sterilizing extracted teeth that contain amalgam. ISO 11143 is an equipment standard for amalgam separators, with defined test methods. Primary removal exposure experiment · DHA CG-10 issue 2, pp. 51 and 69 · Dubai waste-management law · ISO 11143
The Minamata Convention addresses mercury at the level of parties. Its Annex A distinguishes phase-down measures from additional provisions on bulk mercury and use in deciduous teeth, in patients under 15 years, and in pregnant or breastfeeding patients. The latter provision allows a patient-need exception. The UAE’s 2025 national report confirms a group-specific restriction or recommendation but does not identify the implementing UAE measure in that response. For a Dubai clinic, apply the current local rules. The later COP-6 amendment adds 2034 to Annex A for the phase-out of manufacture, import and export of dental amalgam. The Secretariat lists 23 March 2027 as its entry into force for parties that have not notified non-acceptance under the treaty. Minamata Convention text and annexes · UAE 2025 national report, question 4.3(B) · Convention amendment status
Liners, bases and exposed pulp
| Clinical situation | Select the material for the indication |
|---|---|
| Deep caries with dentin still covering a vital pulp | Prioritize the excavation strategy and a well-sealed restoration. The 2026 EFCD–ESE–ORCA guideline suggests against routine cavity lining in this setting. |
| A base or liner is specifically indicated | Use a compatible product over dentin. A base replaces missing dentin and a liner is an interfacial layer. Follow its instructions on site, thickness and cure. A glass ionomer base may be contraindicated for direct pulp contact. |
| Exposed pulp suitable for capping or pulpotomy | Use the specified exposure protocol and a material indicated for direct contact. For permanent teeth with no symptoms or reversible pulpitis and carious exposure, the EFCD–ESE–ORCA guideline favors a hydraulic calcium silicate cement over calcium hydroxide for a cap or pulpotomy. |
Mineral trioxide aggregate (MTA) and tricalcium silicate products such as Biodentine XP are examples of hydraulic calcium silicate cements. Check the actual formulation, set, restoration sequence and follow-up plan. The Biodentine XP instructions report an average setting time of 12 minutes from the end of mixing and note variation. Confirm the material has hardened adequately before the definitive enamel restoration. In DHA CG-01 section B, calcium hydroxide and an RMGI base are specified in its defined mature permanent tooth pulp-capping protocols. Section 12.2 covers exposure selection and other vital pulp therapy evidence. EFCD–ESE–ORCA deep-caries guideline, R2 and R4 · Primary direct pulp capping trial · Biodentine XP instructions · DHA CG-01 section B
A laboratory compares set specimens made from conventional low-copper and a high-copper dental amalgam alloy. Which change explains the decrease in tin–mercury gamma-2 in the high-copper specimen?
Copper reacts with tin to form the eta-prime copper–tin phase.
Copper converts the gamma-1 matrix into glass ionomer.
The high-copper specimen forms more tin–mercury gamma-2.
Phosphoric acid initiates a resin setting reaction.
A cervical root lesion needs restoration. The dentist can retract the gingiva, expose the margin and control contamination. Which material on this list sets with an acid–base reaction and a light-activated resin reaction, can adhere to tooth mineral and can release fluoride?
A conventional light-cured flowable composite.
An unlined high-copper amalgam.
A light-cured resin-modified glass ionomer indicated for cervical restorations.
A hard-setting calcium hydroxide pulp liner.
During caries removal in a permanent molar with findings of reversible pulpitis, an exposure occurs under good isolation. After assessment and bleeding control, vital pulp treatment is selected under the 2026 EFCD–ESE–ORCA guidance. Which material does it favor for direct capping or pulpotomy in this setting?
A conventional luting glass ionomer applied directly over the pulp.
A hydraulic calcium silicate cement with the intended pulp-contact indication.
Zinc oxide–eugenol temporary cement applied to the exposed pulp.
An adhesive alone as a substitute for the pulp dressing.
A Dubai clinic has collected contact and noncontact amalgam waste after clinically indicated restoration removal. What handling does DHA CG-10 issue 2 specify?
Empty the collected material into the sink after use.
Place the waste in general waste bags for routine pickup.
Sterilize the collected amalgam waste by heat before placing it with sharps.
Use airtight containers labeled as biohazard waste and the waste-management unit’s local disposal route.